: Specifications > Tungsten |
|
|
|
|
|
|
|
|
Mn |
<5 |
Mo |
40 |
N
|
<5 |
Na
|
5 |
Nb
|
<5 |
Ni
|
5 |
O
|
<5 |
P
|
20 |
Pb
|
<10 |
S
|
<2 |
Si
|
<10 |
Ti
|
<5 |
W
|
5 |
Zn
|
<5 |
Zr |
<5 |
|
W
|
99.98% |
Ag
|
<5 |
Al
|
10 |
As
|
<1 |
Ba
|
<2 |
C
|
<10 |
Ca
|
5 |
Cd
|
<1 |
Co
|
5 |
Cr
|
<10 |
Cu
|
5 |
Fe
|
20 |
H
|
<1 |
K
|
<5 |
Mg |
<5 |
|
|
|
|
|
|
|
|
|
Properties
|
Unit
|
Tungsten |
Atomic
Weight
|
g/g Atom
|
184 |
Melting
Point
|
°C
|
3,410 |
Density
|
g/cm3 |
19.3 |
Linear
Thermal
Expansion Coefficient |
10-6/K |
20°C |
5.3 |
20~1,000°C |
5.8 |
20~1,500°C |
6.5 |
Specific
Heat |
Joule/g.K |
0.14 |
Thermal
Conductivity |
W/m.K |
129 |
Electrical
Resistance |
m |
0.055 |
|
|
|
|
|
|
|
Properties
|
Unit
|
Molybdenum |
Tensile
Strength |
N/mm2 |
0.5~1.0 thickness (mm) |
1,300 |
1.0~5.0 thickness (mm) |
800 |
Recrystallized |
1,000 |
Compressive
Strength |
N/mm2 |
1,150 |
Modulus
of Elasticity |
KN/mm2 |
410 |
Modulus
of Torsion |
KN/mm2 |
90~22 |
Hardness |
HV30 |
0.5~1.0 thickness (mm) |
500 |
1.0~5.0 thickness (mm) |
460 |
Recrystallized |
360 |
Incipient
Recrystallization |
°C |
1,150 |
Complete
Recrystallization |
°C
|
1,350 |
|
|
|
|
|
|
|
|
|