: Products > Special Metal Division > Molybdenum |
|
|
|
|
|
|
|
|
Mg |
<5 |
Mn |
<5 |
N
|
<5 |
Na
|
<5 |
Nb
|
<5 |
Ni
|
<5 |
O
|
20 |
P
|
<5 |
Pb
|
<5 |
S
|
<5 |
Si
|
5 |
Ti
|
<5 |
W
|
100 |
Zn
|
<5 |
Zr |
<5 |
|
Mo
|
99.97% |
Ag
|
<5 |
Al
|
10 |
As
|
<1 |
Ba
|
<2 |
C
|
15 |
Ca
|
5 |
Cd
|
<1 |
Co
|
5 |
Cr
|
<10 |
Cu
|
5 |
Fe
|
50 |
H
|
<1 |
K
|
<5 |
|
|
|
|
|
|
|
|
|
|
|
Properties
|
Unit
|
Molybdenum |
Atomic
Weight |
g/g Atom |
95.95 |
Melting
Point |
°C |
2620 |
Density |
g/cm3 |
10.2 |
Linear
Thermal
Expansion Coefficient |
10-6/K |
20°C |
5.3 |
20~1,000°C |
5.8 |
20~1,500°C |
6.5 |
Specific
Heat |
Joule/g.K |
20°C |
0.25 |
1,000°C |
0.31 |
2,000°C |
0.44 |
Thermal
Conductivity |
W/m.K |
20°C |
142 |
1,000°C |
105 |
2,000°C |
88 |
Electrical
Resistance |
m |
20°C |
0.052 |
1,500°C |
0.43 |
2,000°C |
0.6 |
|
|
|
|
|
|
|
Properties
|
Unit
|
Molybdenum |
Tensile
Strength |
N/mm2 |
0.10~0.25 thickness (mm) |
785 |
1.51~2.30 thickness (mm) |
645 |
5.01~8.00 thickness (mm) |
590 |
Yield
Strength
(0.2% offset) |
N/mm2 |
0.10~0.25 thickness (mm) |
620 |
1.51~2.30 thickness (mm) |
580 |
5.01~8.00 thickness (mm) |
540 |
Elongation |
% |
0.10~0.25 thickness (mm) |
3 |
1.51~2.30 thickness (mm) |
12 |
5.01~8.00 thickness (mm) |
17 |
Modulus of
Elasticity |
Mpa |
20°C |
320 |
1,000°C |
270 |
Incipient
Recrystallization |
°C |
900 |
|
|
|
|
|
|
|
|
|