: 사양서 > Hastelloy
Typical Analysis in Percent:
Ni (+ Co) bal. Cr 14.5 - 16.5
Fe 4 - 7 Co 2.5

Mo

15 - 17 W 3 - 4.5
C .01 Mn V
Si .08 V .35
Mechanical Properties (at Room Temperature):
  MPa ksi
Ultimate Tensile Strength 790 115
Yield Strength (0.2% offset) 335 52

Elastic Modulus (Tension): 61%

Elastic Modulus (tension):
GPa
10 6 psi
205 29.8

Hardness: 90 HRB
Physical Properties:
Density: 8.89 g/m³
Melting Point/Range: 1325-1370 oC, 2415-2500 ℉

Specific Heat:

J/kg · K

Btu/lb. ·℉
427 0.102

Average Coefficient of Thermal Expansion:

μm/m · K

μin/in · ℉
427 0.102

(Average Value at 25-100 ℃ [75-200 ℉])

Thermal Conductivity:

w/m · K

Btu · in/ft² · h · ℉
9.8 67.9

Electrical Resistivity: 1300 nΩ · m
Curie Temperature: -125 ℃, -193 ℉
Hastelloy is a registered trademark of Hynes International