: 사양서 > Inconel
Typical Analysis in Percent:
Ni 58 min Cr 20 - 23
Fe 5 Co 1

Mo

8 - 10 Nb(+Ta) 3.15 - 4.15
Ti .4 Al .4
C .1 Mn .5
Si .5    
Physical Properties:
Density: 8.44 g/cm3
Melting Point/Range: 1290 - 1350 oC (2350 - 2460 oF)

Specific Heat:
J/kg · K Btu/lb · ℉
1/4 HARD 90,000 TO 115,000

Average Coefficient of Thermal Expansion:
μm/m · K μin./in. · ℉
12.8 7.1

Thermal Conductivity
W/m · K Btu · in./ft² · h · ℉
12.8 7.1

Electrical Resistivity: 1290 nΩ · m
At Room Temperature:
Ultimate Tensile
Strength
Yield Strength
(0.2 % offset)
Elongation in
50 mm (2")
Elastic Modulus
(Tension)
MPa ksi MPa ksi % GPa
10 6 psi

930

135 517 135 42.5 207 30

Hardness: 190 HB
Notice
 
주문 생산 제품 : 필요한 제품을 주문 제작하여 공급합니다.
  필요한 조건과 요구사항등을 첨부하여 연락주십시오.